Aerospace and defense electronic assemblies used in avionics, sensing, communication, navigation, control, mission, and power systems must maintain reliable performance under demanding mechanical, thermal, electrical, and environmental conditions.
Temperature cycling, vibration and shock, moisture, contamination, corrosion, and heat generation can affect components, solder joints, interconnections, and printed circuit board assemblies.
Krayden supports material technologies that protect aerospace and defense electronics at the component, PCB, module, and enclosure level.
Protection Technologies
Protecting Aerospace & Defense Electronics in Harsh Operating Environments
The following operating conditions represent key challenges for aerospace and defense electronics, along with their potential effects and the material protection approaches commonly evaluated for each.
Material Technologies for Aerospace & Defense Electronics Protection
Aerospace and defense electronics rarely rely on a single protection method. A typical assembly may combine conformal coatings for PCB protection, underfill for solder-joint reinforcement, staking for larger components, thermally conductive materials for heat transfer, and sealants around enclosure and connector interfaces.
The right combination depends on the assembly’s operating environment, exposure to vibration and thermal cycling, electrical insulation requirements, heat generation, rework needs, and any program-specific material constraints.

Conformal Coatings
Conformal coatings are used on populated circuit boards to provide thin, lightweight protection against moisture, condensation, contamination, corrosion, and electrical leakage. They are especially useful in aerospace electronic assemblies where environmental protection is needed without fully encapsulating the board or adding significant mass.
Typical Materials
Acrylic, urethane, silicone, UV-curable, and dual-cure coating systems.
Aerospace Function
Protects conductors, solder joints, component leads, and insulating surfaces while allowing connectors, test points, and rework areas to remain selectively uncoated.
Selection Focus
Coating thickness, cure mechanism, shadow-area cure, flexibility, temperature cycling, chemical exposure, inspection method, masking requirements, and reworkability.
Where Used: Avionics PCBs • Radar & Sensor Electronics • Communication & Navigation Assemblies

Encapsulation & Potting
Encapsulation and potting materials surround components or complete assemblies to provide broader protection than conformal coatings. In aerospace electronics, they are often used where assemblies require stronger resistance to moisture, contamination, electrical stress, vibration, and shock, or where added dielectric or thermal performance is needed.
Typical Materials
Epoxy encapsulants, silicone elastomers, polyurethane systems, dielectric gels, and thermally conductive potting compounds.
Aerospace Function
Provides broader environmental and dielectric protection while helping support components against vibration, shock, and handling stresses.
Selection Focus
Modulus, thermal expansion, dielectric properties, thermal conductivity, cure exotherm, weight, operating temperature, and stress on sensitive components.
Where Used: Avionics Modules • Sensors & Connectors • Power Electronics

Underfill
Underfill materials are used beneath surface-mounted packages to reinforce solder interconnections and reduce localized stress. In aerospace electronics, they are especially relevant for assemblies exposed to vibration, thermal cycling, and board flexing, where solder-joint reliability is a key concern.
Typical Materials
Capillary-flow epoxy underfills, reworkable underfills, and specialized low-outgassing underfill systems.
Aerospace Function
Helps redistribute stress away from solder joints and into the package-to-board interface, improving resistance to vibration and repeated thermal expansion mismatch.
Selection Focus
Package geometry, flow behavior, cure temperature, glass transition temperature, modulus, thermal expansion, reworkability, and thermal cycling performance.
Where Used: BGA Packages • High-Density PCBs • Mission & Sensor Electronics

Component Staking & Bonding
Staking and electronic bonding materials help secure larger, taller, or mechanically sensitive components that could otherwise shift under vibration, shock, or repeated loading. In aerospace systems, they are used to reduce stress on leads, solder joints, and connectors and to improve the mechanical stability of the assembly.
Typical Materials
Non-sag epoxy staking compounds, flexible epoxy adhesives, urethane adhesives, and electrically insulating electronic bonding materials.
Aerospace Function
Restrains component movement and transfers mechanical load into the board or adjacent attachment area, reducing repeated loading on leads, solder joints, and connectors.
Selection Focus
Component mass and height, vibration spectrum, shock loading, adhesive flexibility, non-sag behavior, bond geometry, electrical insulation, cure temperature, and repair access.
Where Used: Large Components • Connectors • Vibration-Sensitive PCBs

Thermal Management Materials
Thermal management materials help move heat away from electronic components and into housings, chassis, heat spreaders, or heat sinks. In aerospace electronics, they are important in compact or high-power assemblies where excess heat can affect reliability, performance, and long-term service life.
Typical Materials
Thermally conductive adhesives, gap fillers, thermal tapes, pads, interface materials, and thermally conductive encapsulants.
Aerospace Function
Improves heat dissipation by creating controlled thermal paths across gaps and interfaces while supporting the electrical and mechanical needs of the assembly.
Selection Focus
Thermal conductivity, interface thickness, dielectric performance, compressibility, adhesion, operating temperature, vibration resistance, and thermal cycling.
Where Used: PCB-to-Housing Interfaces • Power Devices • High-Power Modules

Electronic Sealants
Electronic sealants help protect critical interfaces where moisture, contaminants, or other environmental exposure could enter an assembly. In aerospace electronics, they are commonly considered around housings, connectors, cable entries, sensors, and other localized sealing points where flexibility and electrical insulation may be important.
Typical Materials
RTV silicone sealants, controlled-volatility silicones, low-outgassing sealants, and flexible electrically insulating sealing materials.
Aerospace Function
Seals joints and interfaces to help block moisture and contamination while accommodating differential movement, vibration, and thermal expansion.
Selection Focus
Flexibility, elongation, adhesion, dielectric properties, cure chemistry, temperature range, moisture resistance, and low-outgassing requirements where applicable.
Where Used: Housings & Enclosures • Connectors & Cable Entries • Sensors & Optical Assemblies
Aerospace Electronics Protection Materials
Krayden supplies materials from Dow / DOWSIL, HumiSeal, Henkel / LOCTITE, and 3M for aerospace and defense electronic assemblies. These materials support conformal coating, encapsulation, underfill, component staking, thermal management, flexible bonding, electrical insulation, and sealing across PCB, module, sensor, power-electronics, and enclosure applications.

Silicone Protection & Thermal Management for Aerospace and Defense Electronics
DOWSIL materials help aerospace and space electronics manage heat, electrical insulation, environmental exposure, mechanical stress, and material volatility. The products below cover encapsulation, conformal coating, thermal gap filling, thermally conductive bonding, and sealing, including options for low-outgassing and vacuum-sensitive electronic assemblies.

Conformal Coatings for Aerospace PCB Environmental Protection
HumiSeal conformal coatings help protect avionics and other aerospace printed circuit assemblies from moisture, contamination, corrosion, and electrical leakage while adding minimal material around the board. UV40 supports fast UV processing with secondary moisture cure in shadowed areas, while 1B73 provides a fast-drying acrylic coating that supports inspection, repair, and long-term electrical protection.

Component Reinforcement, Underfill & Encapsulation
LOCTITE electronic materials help protect aerospace electronics at the component and package level. ABLESTIK 2112 stabilizes and reinforces PCB components, ECCOBOND UF1173 supports BGA and CSP solder joints during thermal and mechanical loading, and STYCAST 2850FT provides electrically insulating encapsulation where heat dissipation and mechanical protection are both required.

Electrical Protection, Flexible Bonding & Thermal Interfaces
3M materials support aerospace electronic assemblies where electrical insulation, environmental protection, movement, vibration, and heat transfer must be managed. Scotchcast Electrical Resin 281 protects and insulates electrical and electronic components, Scotch-Weld 2216NS provides flexible bonding for assemblies exposed to movement and temperature change, and 8805 creates a thin adhesive thermal path from heat-generating components to cooling structures.
Further Reading on Aerospace Electronics Protection Solutions
Frequently Asked Questions About Aerospace Electronics Protection
Need Help Selecting Materials for Aerospace Electronics Protection?
Material selection depends on the assembly design, operating environment, vibration and shock exposure, temperature range and cycling, moisture or contamination risk, heat generation, electrical requirements, manufacturing process, and applicable aerospace or defense program requirements. Krayden can support material selection, technical data review, and application guidance across conformal coatings, encapsulants, underfills, staking materials, thermal-management materials, and electronic sealants.