Molykote
MOLYKOTE Specialty Lubricants & Lubrication Solutions
MOLYKOTE® is DuPont's specialty-lubricants portfolio for controlling friction, wear, sealing, release, and component movement across automotive and industrial equipment. The portfolio spans greases, oils & fluids, pastes, compounds, anti-friction coatings, and dispersions, with product technologies that include mineral oil, synthetic hydrocarbon, ester, silicone, fluorosilicone, PFPE, and solid-lubricant systems. Depending on the product, MOLYKOTE solutions support bearings, gears, chains, compressors, pumps, valves, seals, threaded connections, electric motors, sliding surfaces, and other demanding lubrication points.
As an authorized MOLYKOTE distributor, Krayden supplies specialty lubricants for equipment design, production, maintenance, and repair applications. Our team can help compare lubricant type, base chemistry, viscosity or consistency, load, speed, temperature, environmental exposure, material compatibility, and application method so customers can narrow the appropriate MOLYKOTE options for a specific operating condition.
Markets Served by MOLYKOTE
Greases
MOLYKOTE greases combine a lubricating fluid, thickener, and performance additives or solid lubricants to stay in place where a flowing oil is not practical. The portfolio spans general machinery lubrication, high-load and severe-duty service, wide-temperature applications, chemically demanding environments, and low-noise or precision-bearing duties. Selection should account for load, environment, temperature, speed, relubrication interval, base-oil chemistry, thickener system, and compatibility with nearby metals, plastics, elastomers, or process media.
Oils & Fluids
MOLYKOTE oils and fluids provide flowing lubrication for gears, gearboxes, pumps, chains, compressors, vacuum equipment, slides, and other machinery where circulation, penetration, or controlled fluid delivery is preferred over a grease. The portfolio includes mineral and synthetic base-fluid technologies. Selection should consider viscosity, operating temperature, load and speed, oxidation or corrosion exposure, equipment design, material compatibility, and any process-specific requirements.
Pastes
MOLYKOTE pastes are greaselike lubricants with a high concentration of solid lubricants for assembly, running-in, anti-seize, and heavily loaded metal contact. They are commonly considered for threaded connections, press fits, splines, gears, and other slow-moving or startup contacts where the carrier oil may be displaced but a solid lubricating film is still needed. Product selection should consider substrate metallurgy, load, temperature, corrosion exposure, required friction behavior, and assembly or disassembly requirements.
Compounds
MOLYKOTE compounds are greaselike silicone-based materials used where lubrication and sealing, release, electrical insulation, moisture resistance, or compatibility with rubber and plastics may be required. The category extends beyond release compounds to include valve and seal lubrication, O-ring assembly, dielectric moisture barriers, noncuring sealing functions, and selected plastic or elastomer lubrication duties. Confirm product-specific compatibility and any regulatory or process requirements for the intended application.
Anti-Friction Coatings
MOLYKOTE anti-friction coatings are bonded dry-film lubricants containing solid lubricants dispersed in resin and solvent systems. After application and curing, they form a thin lubricating film on the component surface and are used where a clean, dry lubricant is preferred, where dust or contamination makes wet lubrication undesirable, or where relubrication access is limited. Coating choice depends on substrate, surface preparation, application method, cure requirements, film thickness, load, motion, and service environment.
Dispersions
MOLYKOTE dispersions suspend finely divided solid lubricants in a liquid carrier so the lubricant can be applied by liquid methods, including automatic dispensing where appropriate. They are used for dry-film lubrication of sliding contacts, lubrication of chains, conveyors and bearings in demanding temperature conditions, selected cutting or sewing operations, release applications, and other specialty processes. Selection should consider carrier chemistry, evaporation or residue behavior, application equipment, surface material, required film, temperature, and process compatibility.
Talk to our Experts
Whether you are comparing a grease, oil, paste, compound, coating, or dispersion, Krayden can help narrow MOLYKOTE options around the actual lubrication point. Our team can support product comparison, application requirements, load-speed-temperature review, material compatibility, environmental exposure, and practical application or maintenance considerations.
MOLYKOTE Quick Reference
244 products
-
MOLYKOTE 3451
- Fluorosilicone Grease Formulation
- 40 to 450 deg F Service Range
- 340 kg Four-Ball Weld Load
-
MOLYKOTE 7
- 40 to 204 deg C Service Range
- Release, Lubrication, Sealing, and Protection
- 0.8% Evaporation at 200 deg C
-
MOLYKOTE D-321R AN-FR
- Room-Temperature Application Cure
- Dry Film Lubricant Formulation
- 180 to 450 deg C Service Range
-
MOLYKOTE EM-D110
- Compatible with Most Plastics
- High-Viscosity PAO Oil
- Silicone-Free Lubrication Formulation
-
MOLYKOTE G-2008
- Fully Synthetic PAO-Based Grease with Lithium Thickener
- Manual or Automated Dispensing
- Sub-0.55 mm Four-Ball Wear
-
MOLYKOTE G-68
- Good Compatibility with Most Plastics
- 0.014 Coefficient of Friction
- Water-Resistant Grease Lubrication
-
MOLYKOTE G-N METAL ASSEMBLY PASTE
- Heavy-Duty Assembly Paste
- 0.08 Coefficient of Friction
- Metal Interfaces Protection
-
MOLYKOTE HI-VAC SILICONE BASED HIGH VACUUM GREASE
- Low-Volatility Silicone Grease
- Less Than 0.5% Bleed
- Seals and Lubricates Vacuum and Pressure Systems
-
DUROPTIX OE-6370
- 1:1 Optical Encapsulant Mixing
- 100% Transparent Optical Protection
- 240-Minute 150 deg C Cure
-
-
ECCOSORB AN-77
- Carbon Loaded, Multilayer Absorber
- Broadband Free Space Absorber
- Low-Weight RF Absorber
-
-
LAIRD JCP-PP9
- 60+ GHz Injection-Moldable Absorber
- 76 to 81 GHz Automotive Radar Use
- Polypropylene-Like Mechanical Integration
-
-
LAIRD MCS/SS6M
- 800 MHz to 6 GHz Absorption
- Low-Outgassing Silicone Construction
- Flexible Sheet with Optional PSA
-
LAIRD TPUTTY 502FG2
- 3.0 W/(m K) Thermal Interface
- Ultra-Soft 14 Shore 00 Material
- Thermal Interface Material
-
LAIRD VY-81
- 80 to 90 dB EMI/RF Shielding
- Non-Hardening High-Tack Shielding Compound
- Conventional Caulking-Equipment Application
-
MOLYKOTE 1000
- No Intentional PFAS, Lead, or Nickel
- -30 to 650 deg C Service Range
- Consistent Friction and High Load Capacity
-
MOLYKOTE 106
- Heat-Curing Dry Film Lubricant
- High-Load Coating Application
- 70 to 250 deg C Service Range
-
-
MOLYKOTE 1122
- High-Viscosity Lubricant Formulation
- Robust High-Pressure Resistance and Wear Protection
- High-Temperature Lubrication Protection
-
MOLYKOTE 3099
- Water-Repellent High-Voltage Insulator Coating
- 800-Minute ASTM D2303 Arc Resistance
- Hand, Pad, Brush, or Spray Renewal
-
MOLYKOTE 316
- Effective, Heat-Stable Anti-Stick Silicone Film
- FDA 21 CFR 175.300 Compliance
- Oxidative Breakdown Resistance
-
MOLYKOTE 3179
- Dilatant Rheological Behavior
- Non-Slumping Static-Flow Resistance
- Novelty/Educational Toy-Market Use
-
MOLYKOTE 33
- NLGI 2 Silicone Grease
- Water-Resistant Light-Load Lubrication
- 73 to 180 deg C Service Range
-
MOLYKOTE 3400A
- 30-Minute 200 deg C Heat Cure
- High-Load Dry-Film Wear Resistance
- 500-Hour Red-Rust Resistance
-
MOLYKOTE 3452
- Multi-Solvent Chemical Resistance
- Defined 8-Hour Exposure Testing
- 400 kg Four-Ball Weld Load
-
-
MOLYKOTE 41
- Silicone Oil Base and Carbon Black Thickener
- 20 to 290 deg C Service Range
- Water and Oxidation Resistance
-
-
MOLYKOTE 5
- Nonconductive, Water-Repellent Silicone Paste
- 54 to 232 deg C Service Range
- Metal and Plastic Compatibility
-
MOLYKOTE 55
- Silicone Base Oil and Lithium Soap Thickener
- Heat-Stable Oxidation-Resistant Grease
- D4/D5/D6 Cyclic-Siloxane Compliance
-
MOLYKOTE 557
- Clear Nonstaining Wax-Like Film
- 0.07 Coefficient of Friction
- Federal Meat/Poultry Program Authorization
-
MOLYKOTE 7400
- Water-Based MoS2/Graphite Dry-Film Lubricant
- High Load-Carrying Capacity
- Air-Curing Lubricant Coating
-
MOLYKOTE 7415
- Molykote D-7405, D-7409, and D-7620 Anti-Friction Coatings
- Low Evaporation Rate
- PTFE- and PFAS-Free Formulation
-
MOLYKOTE BG20
- 45 to 180 deg C Service Range
- 2,400 N Four-Ball Weld Load
- Manual or Automated Dispensing
-
MOLYKOTE BG-555
- Low-Noise Bearing Grease
- Water-Washout and Corrosion Resistance
- -40 to 150 deg C Service Range
-
MOLYKOTE BR-2
- MoS2/Graphite Lithium Grease
- High-Load Moderate/High-Speed Lubrication
- Long-Term Industrial Lubrication
-
MOLYKOTE CU-7439
- Up to 650 deg C Service
- High-Adhesion Copper Paste
- Nondestructive Thread-Disassembly Support
-
-
-
-
MOLYKOTE D-7409
- Heat-Curing Dry-Film Lubricant
- High-Load Wear-Resistant Dry-Film Lubrication
- Solvent and Oil Resistance
-
MOLYKOTE D-96
- Transparent Water-Based PTFE Dry Film
- 100,000-Cycle No-Noise Pairing Result
- -40 to 150 deg C Service Range
-
MOLYKOTE DX
- 4,800 N Four-Ball Weld Load
- 0.10 Press-Fit Friction Coefficient
- -25 to 125 deg C Service Range
-
MOLYKOTE EM-30L
- -45 to 150 deg C Service Range
- 3,730 N Four-Ball Weld Load
- 0.4% Evaporation at 99 deg C
-
MOLYKOTE EM-50L
- Broad Plastic Compatibility
- 100% Silicone-Free PAO Grease
- Low-Seepage Long-Service Lubrication
-
MOLYKOTE E-PASTE
- 560 kg Four-Ball OK Load
- ABS, Polycarbonate, Nylon, Polyacetal Compatibility
- -50 to 150 deg C Service Range
-
MOLYKOTE G-0010
- Polyurea-Thickened Mineral-Oil Grease
- Above 260 deg C Dropping Point
- Corrosion-Preventive Bearing Grease
-
-
MOLYKOTE G-0052
- FDA 21 CFR 178.3570 Compliance
- 6,080 N Four-Ball Weld Load
- Water-Resistant Grease Lubrication
-
-
MOLYKOTE G-1067
- Low-Friction Plastic-Compatible PAO Grease
- 50 to 120 deg C Service Range
- Automotive Lubrication Applications
-
MOLYKOTE G-1502FM
- Oil and Water Resistance
- FDA 21 CFR 178.3570 Compliance
- 40 to 149 deg C Service Range
-
MOLYKOTE G-3000
- Dual-Mass-Flywheel High-Shear Grease
- -40 to 180 deg C Service Range
- 2,200 N Four-Ball Weld Load
-
MOLYKOTE G-3407
- -40 to 200 deg C Service Range
- Brake-Caliper Guide-Pin Lubrication
- 120-Hour No-Rust Test Result
-
MOLYKOTE G-4500FM
- 40 to 150 deg C Service Range
- 18 kg Four-Ball Weld Load
- NLGI 2 PAO/Aluminum-Complex Grease
-
MOLYKOTE G-4501
- FDA 21 CFR 178.3570 Compliance
- Lower-Consistency (NLGI 1) PAO Synthetic Grease
- 40 to 150 deg C Service Range
-
MOLYKOTE G-4700
- Extreme-Load Bearing Lubrication
- PAO Synthetic Base Oil and Lithium Complex Thickener
- Industrial Plastic/Elastomer Compatibility
-
-
MOLYKOTE G-5042
- Effective Purple Silicone Grease
- Siloxane Base Oil and Lithium Soap Thickener
- Long-Term Silicone-Grease Lubrication
-
MOLYKOTE GN
- Mineral-Oil Solid-Lubricant Assembly Paste
- 0.08 Press-Fit Friction Coefficient
- 2,800 N Four-Ball Weld Load
-
MOLYKOTE HP-300
- Fully Fluorinated PFPE/PTFE Lubrication
- 65 to 250 deg C Service Range
- 3,300 N Four-Ball Weld Load
-
MOLYKOTE HP-870
- Fully Fluorinated Formulation
- -20 to 250 deg C Service Range
- Chemical-Resistant PFPE/PTFE Grease
-
MOLYKOTE L-1268
- Fully Synthetic ISO Vg 68 PAO Lubrication
- 54 deg C Pour Point
- Longer Oil-Drain Intervals
-
MOLYKOTE L13
- Adjusts the Application Viscosity
- Compatible Cleaning Solvent
- Defined Range of Molykote Coatings
-
-
-
MOLYKOTE LONGTERM 2 PLUS
- 3,800 N Four-Ball Weld Load
- Heavily Loaded Metal-to-Metal Components Protection
- 25 to 110 deg C Service Range
-
MOLYKOTE M-77
- Up to 400 deg C Service
- Silicone Carrier Oil
- Selected Metal, Plastic, Rubber, and Elastomer Contacts
-
MOLYKOTE P37
- -30 to 1400 deg C Threaded-Connection Lubrication
- 5,500 N Four-Ball Weld Load
- Graphite/Zirconium-Dioxide High-Purity Paste
-
MOLYKOTE P-40
- Metal-Free Lubrication Paste
- Assembly and Continuous Lubrication
- -40 to 121 deg C Paste Service
-
MOLYKOTE PA-744
- 10 to 20 um Screen-Printed Film
- High-Wear High-Load Dry Lubrication
- -75 to 300 deg C Service Range
-
MOLYKOTE PG54
- Long-Term Lubrication for Metal-to-Plastic
- 50 to 180 deg C Service Range
- Silicone Base Oil
-
MOLYKOTE TP-42
- 3,000 N Four-Ball Weld Load
- Water-Resistant Grease Lubrication
- Stick-Slip, Galling, and Corrosion Protection
-
MOLYKOTE YM103
- PAO/PTFE Lubrication for Plastic-on-Plastic
- 45 to 150 deg C Service Range
- Automotive Lubrication Applications
-
MOLYKOTE Z-POWDER
- 98% MoS2 Solid Lubricant
- 185 to 400 deg C Service Range
- 0.048 Coefficient of Friction
-
LAIRD LS-30
- Compliant Polyurethane Foam Format
- RF Isolation and Insertion Loss
- Cavity Resonance Suppression
-
-
-
LAIRD RFLB/SS6M
- Adhesive-Backed 0.51 mm Sheet
- 10 MHz to 4 GHz Control
- Greater Than 50 dB/cm Attenuation
-
MOLYKOTE BG-20
- DN 750,000 High-Speed Operation
- Medium-to-Heavy Load Lubrication
- -45 to 180 deg C Service
-
-
-
MOLYKOTE G684OZTUBES
- Plastic Gear Friction Control
- 75 mm2/s Base Oil
- Brush-to-Central System Application
-
-
-
-
-
-
ECCOSORB SF-5.5
- 5.5 GHz Absorber Tuning
- 163 deg C Maximum Operating Temperature
- PSA or On-Drawing Options
-
ECCOSORB SF-6.0
- 6.0 GHz Absorber Tuning
- 163 deg C Maximum Operating Temperature
- PSA or On-Drawing Options
-
ECCOSORB SF-7.0
- 7.0 GHz Absorber Tuning
- 163 deg C Maximum Operating Temperature
- PSA or On-Drawing Options
-
ECCOSORB SF-8.5
- 8.5 GHz Absorber Tuning
- 163 deg C Maximum Operating Temperature
- PSA or On-Drawing Options
-
LAIRD BSR
- 6-18 GHz cavity-resonance control
- Flexible, electrically non-conductive silicone construction
- 0.47% TML / 0.28% CVCM outgassing values
-
LAIRD CF500
- X/Y/Z-axis conductive foam for EMI shielding and grounding
- Low-compression gasket design with a typical 25-50% operating compression range
- One-sided conductive PSA with die-cut, hole-punch, and notch customization
-
LAIRD F2R2/PSA
- Fuel-Resistant Microwave Absorption
- Up-to-475-deg-F Temperature Capability
- PSA-Backed Aerospace Configurations
-
LAIRD LS-30/SS3
- High-Loss LS-30 Microwave Grade
- Flexible Conductive Foam Construction
- SS3 Pressure-Sensitive Adhesive Backing
-
LAIRD MFS-124
- 6-to-35-GHz Microwave Absorption
- Flexible Non-Conductive Silicone Sheet
- Good Fit for RF Structures
-
LAIRD NS1000
- Three Tuned Permeability Sub-Series
- Ultrathin Near-Field EMI Suppression
- Flexible PSA-Optional Sheet Formats
-
LAIRD NS1000C
- 110 Initial Permeability at 1 MHz
- 20-MHz-to-3-GHz Noise Suppression
- Thin Flexible PSA-Optional Formats
-
LAIRD RFRET-0
- Lightweight Broadband Foam Absorption
- 2-to-18-GHz Reflection Reduction
- Flexible Multi-Method Attachment
-
LAIRD SF4.5
- 4.5 GHz Narrow-Band Absorption
- Flexible Metal-Surface Conformability
- 163 deg C Service Capability
-
LAIRD SF-9.0/SS6M
- 9 GHz Resonant Reflection Control
- Thin 1.73 mm Sheet Format
- 163 deg C Maximum Service Temperature
-
LAIRD TPUTTY 508
- One-Part Automated Dispensing
- Vertical Gap-Filler Stability
- 3.7 W/(m K) Thermal Transfer
-
MOLYKOTE 211
- Heat-Stabilized Shear Viscosity
- Blendable Viscosity Grade Range
- Automotive Fan-Clutch Fluid
-
-
MOLYKOTE 7325
- Starter-Motor Clutch Lubrication
- -40 to 150 deg C Range
- Oxidation and Moisture Resistance
-
MOLYKOTE 7365
- Friction-Stabilizing Brake Formulations
- 3 to 7 Weight-Percent Blending
- Up to 650 deg C Application
-
MOLYKOTE 7375
- Multipurpose Brake-Pad Addition
- 3 to 7 Weight-Percent Blending
- Up to 650 deg C Application
-
MOLYKOTE AG-633
- Plastic-Compatible PAO Lubrication
- -50 to 150 deg C Range
- Non-Silicone Grease Formulation
-
MOLYKOTE AI-6159
- Automotive Plastic Noise Control
- Window-Regulator Guide Lubrication
- -40 to 150 deg C Range
-
-
MOLYKOTE G-0051 FM
- NSF H1 Incidental-Contact Lubrication
- High-Load NLGI 1 Grease
- Food-Machinery Bearing Coverage
-
MOLYKOTE G-0102
- Water-Resistant Bearing Lubrication
- Extreme-Pressure Load Support
- Heavy-Industry Moisture Service
-
MOLYKOTE G-1041
- Plastic-Compatible Synthetic Lubrication
- -60 deg C Low-Temperature Operation
- Low-Evaporation PAO Grease
-
MOLYKOTE G-1056
- Automotive Noise-Reduction Lubrication
- No-Oil-Bleed PAO Formulation
- Power Slide-Door Coverage
-
MOLYKOTE G-4000
- NLGI 00 Automatic Dispensing
- NSF H1 Incidental-Contact Lubrication
- Multipurpose Machine-Element Coverage
-
MOLYKOTE G-407
- Brake-Caliper Guide-Pin Lubrication
- Metal-to-Metal Fretting Control
- -40 to 150 deg C Range
-
-
MOLYKOTE G-804
- Nonmelting High-Temperature Lubrication
- Moisture-Resistant Seal Lubrication
- Rubber and Plastic Component Coverage
-
MOLYKOTE G-807
- Low-Friction Electromechanical Lubrication
- Plastic and Rubber Compatibility
- -40 to 150 deg C Range
-
-
MOLYKOTE L-0268
- Corrosion-Inhibited Process-Gas Lubrication
- ISO 68 Compressor-Oil Selection
- Controlled Oxygen-Service Boundary
-
MOLYKOTE L-0322
- ISO 22 Hydraulic-Fluid Selection
- Rust-Oxidation and Anti-Wear Additives
- Low-Viscosity Hydraulic System Service
-
MOLYKOTE L-0346
- ISO 46 Hydraulic-Fluid Selection
- Rust-Oxidation and Anti-Wear Additives
- Medium-Viscosity Hydraulic System Service
-
-
MOLYKOTE L-1122FM
- NSF H1 Food-Machinery Lubrication
- ISO 220 PAO Gear Lubrication
- High-Load Oxidation Resistance
-
-
MOLYKOTE L-1146FM
- High-Viscosity Gearbox Lubrication
- PAO Viscosity Index 152
- Food-Processing Gear Service
-
MOLYKOTE L-1210
- ISO VG 100 Compressor Lubrication
- PAO Wide-Temperature Viscosity
- Rust and Oxidation Protection
-
-
MOLYKOTE L-1232FM
- ISO VG 32 Compressor Lubrication
- PAO Low-Temperature Flow
- Food-Grade Compressor Oil Identity
-
MOLYKOTE L-1246
- ISO VG 46 Compressor Lubrication
- PAO Low-Temperature Flow
- Rust and Oxidation Protection
-
MOLYKOTE L-1246FM
- NSF H1 Compressor Lubrication
- Temperature-Indexed PAO Viscosity
- Food-Machinery Lubrication Scope
-
MOLYKOTE L-1428
- High-Temperature Chain Lubrication
- High-Viscosity Chain-Oil Profile
- Rust and Anti-Wear Additives
-
MOLYKOTE L-1510
- Corrosive-Gas Compressor Lubrication
- Wide-Range ISO VG 100 Stability
- Clear Oxygen-Service Boundary
-
MOLYKOTE L-1568
- Lower-Viscosity Process-Gas Lubrication
- Wide-Range PAO Viscosity Control
- Defined Oxygen-Service Limit
-
MOLYKOTE L-2115
- Extreme-Pressure Enclosed-Gear Lubrication
- Micropitting-Focused PAO Protection
- Rapid 10-Minute Water Separation
-
MOLYKOTE L-2122
- Stable ISO VG 220 Gear Lubrication
- Micropitting Protection in Severe Conditions
- High FZG Load-Carrying Performance
-
MOLYKOTE L-2132
- High-Viscosity Enclosed-Gear Lubrication
- Corrosion-Inhibited EP Formulation
- Severe-Condition Micropitting Protection
-
MOLYKOTE L-3246
- Wide-Temperature PAG/POE Viscosity
- Oxidation-Resistant Compressor Lubrication
- Rotary-Screw Compressor Fit
-
MOLYKOTE L-4611
- Dedicated Reciprocating-Compressor Lubrication
- Temperature-Indexed Diester Viscosity
- Rust and Oxidation Protection
-
MOLYKOTE L-8030
- Non-Sticky Semi-Dry Lubrication
- Tested Plastic-Contact Compatibility
- Low-Friction Sliding Performance
-
MOLYKOTE MH-62
- Compatible Plastic-Contact Lubrication
- Broad-Range PAO Grease Performance
- Solid-Lubricant Load Support
-
MOLYKOTE MI-60
- Plastic-Compatible Long-Term Lubrication
- Wide-Temperature Mechanical Lubrication
- High-Load Grease Performance
-
MOLYKOTE P-1500
- Assembly and Long-Term Lubrication
- Heavy-Load Sliding Contact Protection
- Wide-Temperature Metallic Component Use
-
MOLYKOTE P-37
- Extreme-Heat Fastener Protection
- High-Load Anti-Seize Performance
- Low-Seepage Clean Assembly
-
MOLYKOTE PG21
- Wide-Temperature Plastic Lubrication
- Oxidation-Resistant Silicone Grease
- Water-Resistant Friction Contact Lubrication
-
MOLYKOTE PG65
- High-Speed Electromechanical Lubrication
- Plastic and Rubber Interface Fit
- Low-Friction Contact Performance
-
MOLYKOTE PG75
- Low-Temperature Plastic Lubrication
- Very Low Friction Performance
- Long-Term Automotive Mechanism Use
-
MOLYKOTE YM102
- Mixed-Material Sliding Lubrication
- Wide-Temperature PAO Grease
- Low-Seepage Precision Equipment Use
-
LAIRD CF600
- X/Y/Z-axis conductive foam for EMI shielding and grounding
- Low-compression gasket design with a typical 25-50% operating compression range
- One-sided conductive PSA with die-cut, hole-punch, and notch customization
-
-
LAIRD TPUTTY SF560
- 5.6 W/m-K Non-Silicone Putty
- 60 g/min Cartridge Flow
- Low-Fogging Reworkable Interface
-
LAIRD TPCM910
- Phase Change Near 50 deg C
- Naturally Tacky Without Added Adhesive
- Pressure-Qualified Thermal Impedance
-
-
LAIRD TPCM780SP
- Screen-Printable Non-Silicone Paste
- 5.4 W/m-K Dry-State Conductivity
- 25 Micrometer Minimum Bondline
-
-
LAIRD SNL60RXP
- 100 dB 200 MHz to 10 GHz Shielding
- 1-Hour Room-Temperature Handling
- -50 to 125 deg C Service Range
-
LAIRD TFLEX 3130
- 3.25 mm Tflex 300 Gap Filler
- Greater Than 50% Deflection at 50 psi
- 1.2 W/(m K) Thermal Conductivity
-
LAIRD TFLEX 300
- Over 50% Deflection at 50 psi
- 1.2 W/(m K) Thermal Conductivity
- 0.50 to 5.08 mm Thickness Range
-
-
LAIRD TFLEX 640
- 1.02 mm Thickness of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Naturally Tacky Surfaces
-
LAIRD TFLEX 6150
- 3.75 mm Thickness of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Naturally Tacky Surfaces
-
LAIRD TFLEX 680
- 2.03 mm Thickness of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Naturally Tacky Pad Surfaces
-
LAIRD TFLEX 660
- 1.50 mm Medium-Gap of Tflex 600 Series
- 3.0 W/(m K) Thermal Interface
- Easy Assembly and Placement with Naturally Tacky
-
LAIRD TFLEX HD90500
- 7.5 W/(m K) Thermal Interface
- Compliant Silicone Gap Filler
- Naturally Tacky Construction
-
LAIRD TFLEX HD91000
- 1.00 mm Controlled-Compression Pad
- 7.5 W/mK Thermal Conductivity
- 0.20 C-in2/W at 10 psi
-
LAIRD TFLEX HD93500
- 7.5 W/(m K) Thermal Interface
- Compliant Silicone Gap Filler
- Naturally Tacky Construction
-
LAIRD TGON 805
- 0.13 mm Flexible Graphite Interface
- 5 W/(m K) Through-Plane Conductivity
- 0.07 deg C in^2/W Thermal Resistance
-
-
LAIRD TFLEX 6110
- 3 W/mK Thermal Conductivity
- Greater Than 90% Recovery
- Naturally Tacky Adhesive-Free Placement
-
LAIRD TFLEX 320H
- Dry Preformed Interface Pad
- No Mixing or Dispensing
- Controlled-Compression Gap Filling
-
LAIRD TFLEX 3200
- Low-Pressure Compliant Gap Filling
- Tgard Dielectric Handling Layer
- Reusable Low-Compression-Set Pad
-
LAIRD TFLEX 3160
- 4.06 mm Gap-Filling Format
- Over-50% Compressive Deflection
- Low-Pressure Thermal Transfer
-
LAIRD TFLEX SF10.0.50
- 0.50 mm Thin-Gap Format
- 10.2 W/m-K Thermal Conductivity
- Non-Silicone Electrical Insulation
-
LAIRD TFLEX SF10
- 10 W/m-K Non-Silicone Interface
- Low-Pressure Thermal Contact
- 0.3 to 5.0 mm Sheet Range
-
LAIRD COOLZORB-500
- Dual Thermal and EMI Management
- Broadband 1-to-90-GHz EMI Suppression
- Compliant Low-Stress Interface Contact
-
LAIRD TFLEX HP34
- 34 W/m-K Bulk Conductivity
- Low Contact Resistance Under Pressure
- Non-Silicone Aligned-Graphite Construction
-
-
LAIRD TFLEX HD93000
- 3.00 mm High-Deflection Pad
- 7.5 W/mK Thermal Conductivity
- Low-Outgassing Silicone Interface
-
LAIRD A10095-02
- High-Conductivity Thermal Gap Filling
- Soft Compliant Interface Contact
- Single-Side Adhesive Placement
-
LAIRD TPUTTY 506
- No-Cure Single-Part Putty
- 3.5 W/m-K Thermal Conductivity
- Low-Pressure Uneven-Gap Filling
-
-
LAIRD TFLEX 3180TG
- Cut-Through-Resistant Dielectric Barrier
- Mass-Production Handling Support
- Compliant 4.57 mm Gap Filling
-
LAIRD TFLEX 3140
- 3.56 mm Gap-Filling Thickness
- High-Compliancy Interface Contact
- Reusable Low-Compression-Set Pad
-
LAIRD TFLEX 320FG
- Thin 0.51 mm Reinforced Interface
- 20 Mil Thickness-Specific Hardness
- Low-Compression-Set Pad Reuse
-
LAIRD TFLEX 340
- 40 Mil Low-Pressure Thermal Resistance
- High-Compliancy Interface Coverage
- Reusable Low-Compression-Set Pad
-
LAIRD TFLEX 350
- 1.25 mm Gap-Filling Thickness
- Compliant Low-Pressure Heat Transfer
- Reusable Low-Compression-Set Pad
-
LAIRD TFLEX 370TG
- Cut-Through-Resistant Tgard Barrier
- Mass-Production Part Handling
- Compliant 1.75 mm Gap Filling
-
LAIRD TFLEX 380
- 2.03 mm Preformed Gap Filling
- Over-50% Deflection at 50 psi
- Low-Compression-Set Pad Reuse
-
LAIRD TFLEX 540
- 0.040-Inch Gap-Filler Format
- 2.8 W/(m K) Thermal Transfer
- Compliant Low-Pressure Interface Contact
-
LAIRD TFLEX 560
- 0.060-Inch Gap-Filler Format
- 2.8 W/(m K) Thermal Transfer
- Naturally Tacky Adhesive-Free Placement
-
LAIRD TFLEX 6100
- 0.100-Inch Gap-Filler Format
- 3.0 W/(m K) Thermal Transfer
- Compliant Low-Stress Interface Contact
-
LAIRD TFLEX 6120
- 0.120-Inch Gap-Filler Format
- 3.0 W/(m K) Thermal Transfer
- Naturally Tacky Adhesive-Free Placement
-
LAIRD TFLEX 6130
- 0.130-Inch Gap-Filler Format
- Compliant Low-Stress Interface Contact
- Electrically Insulating Thermal Interface
-
LAIRD TFLEX 6160
- 0.160-Inch Gap-Filler Format
- Highly Compliant Low-Stress Contact
- Naturally Tacky Adhesive-Free Placement
-
LAIRD TFLEX 6200
- Maximum 0.200-Inch Standard Format
- 3.0 W/(m K) Thermal Transfer
- Compliant Adhesive-Free Interface Placement
-
LAIRD TFLEX 630
- Thin 0.030-Inch Gap-Filler Format
- Compliant Low-Stress Interface Contact
- Naturally Tacky Adhesive-Free Placement
-
LAIRD TFLEX 650
- 0.050-Inch Gap-Filler Format
- 3.0 W/(m K) Thermal Transfer
- Compliant Adhesive-Free Interface Placement
-
LAIRD TFLEX 670
- 0.070-Inch Gap-Filler Format
- Electrically Insulating Thermal Interface
- Compliant Adhesive-Free Interface Placement
-
LAIRD TFLEX 720
- 0.020-Inch Preformed Gap Control
- 5 W/(m K) Interface Heat Transfer
- Naturally Tacky Assembly Placement
-
LAIRD TFLEX 7200
- 0.200-Inch Preformed Gap Control
- Compliant Low-Pressure Heat Transfer
- Electrically Insulating Gap Pad
-
LAIRD TFLEX 740
- 0.040-Inch Preformed Gap Control
- High-Compliancy Surface Conformance
- Wide -40 to 200 deg C Operation
-
LAIRD TFLEX 760
- 0.060-Inch Preformed Gap Control
- Low-Pressure Thermal Resistance
- Naturally Tacky Interface Placement
-
LAIRD TFLEX B2120
- 0.120-Inch Preformed Gap Control
- Compliant Low-Modulus Interface
- 2 W/(m K) Interface Heat Transfer
-
LAIRD TFLEX B240
- 0.040-Inch Preformed Gap Control
- 2 W/(m K) Interface Heat Transfer
- High-Resistivity Electrical Insulation
-
LAIRD TFLEX B260
- 0.060-Inch Preformed Gap Control
- Compliant Low-Modulus Gap Filling
- Reinforced Handling Options
-
LAIRD TFLEX HD320
- 0.020-Inch Variable-Gap Interface
- Low-Pressure High-Deflection Gap Filling
- Low-Resistance Surface Wetting
-
LAIRD TFLEX HD340
- 0.040-Inch Variable-Gap Interface
- Low 0.573 deg C in^2/W Resistance
- High-Deflection Tolerance Accommodation
-
LAIRD TFLEX HD350
- 0.050-Inch Variable-Gap Interface
- 2.7 W/(m K) Interface Heat Transfer
- Low-Pressure High-Deflection Conformance
-
LAIRD TFLEX HD360
- Low-Pressure Variable-Gap Conformance
- 2.7 W/(m K) Thermal Transfer
- 0.060-Inch Thickness Control
-
LAIRD TFLEX HD380
- 80-Mil Variable-Gap Coverage
- Low-Resistance Surface Wetting
- Low-Stress Board Interface
-
LAIRD TFLEX HD7100
- 5.0 W/(m K) Gap Bridging
- Low-Stress Interface Compression
- 0.100-Inch Thickness Selection
-
LAIRD TFLEX HD730
- Thin 0.030-Inch Gap Control
- 5.0 W/(m K) Thermal Path
- Low-Pressure Component Interface
-
LAIRD TFLEX HD740
- Surface-Wetting Contact Performance
- Low-Resistance Thermal Interface
- 0.040-Inch Thickness Selection
-
LAIRD TFLEX HD760
- Reduced Component-Load Conformance
- 5.0 W/(m K) Heat Transfer
- 0.060-Inch Gap-Filler Grade
-
LAIRD TFLEX HD91250
- 7.5 W/(m K) Thermal Transfer
- Low-Outgassing Thermal Interface
- 1250-um Thickness Precision
-
LAIRD TFLEX HD91500
- High-Conductivity Gap Bridging
- Low-Pressure Surface Conformance
- 1500-um Thickness Availability
-
LAIRD TFLEX HR460
- Low-Modulus Interface Conformance
- High-Recovery Reassembly Performance
- Naturally Tacky Placement Control
-
LAIRD TFLEX HR480
- 80-Mil Tolerance Bridging
- Recovery Through Device Rework
- Adhesive-Free Placement Tack
-
LAIRD TFLEX HR630
- High-Recovery Gap Conformability
- 3.0 W/(m K) Thermal Conductivity
- 30 Mil Controlled Thickness
-
LAIRD TFLEX HR640
- Pressure-Qualified Thermal Resistance
- High-Recovery Gap Conformability
- 40 Mil Controlled Thickness
-
LAIRD TFLEX P130
- Shore 00 13 Conformability
- Integrated Tgard Handling Liner
- 30 Mil Controlled Thickness
-
LAIRD TFLEX P180
- 80 Mil Wide-Gap Coverage
- Pressure-Qualified Thermal Resistance
- Soft Tgard-Lined Conformability
-
LAIRD TFLEX P380
- Polyimide-Lined Electrical Isolation
- 3.0 W/(m K) Thermal Conductivity
- Pressure-Qualified Thermal Resistance
-
LAIRD TFLEX SF620
- Non-Silicone Thermal Interface
- 3.0 W/(m K) Thermal Conductivity
- 20 Mil Compact Profile
-
LAIRD TFLEX SF890
- 7.8 W/(m K) Thermal Conductivity
- Non-Silicone Thermal Interface
- 90 Mil Wide-Gap Coverage
-
LAIRD TPLI210FG
- Fiberglass-Reinforced Thin Profile
- 6.0 W/(m K) Thermal Conductivity
- Selectable A0 And A1 Configurations
-
LAIRD TPLI2110
- Compliant 0.110-Inch Gap Filling
- 6.0 W/(m K) Interface Conductivity
- Electrically Insulating Thermal Path
-
LAIRD TPLI2160
- 0.160-Inch Gap Accommodation
- 6.0 W/(m K) Thermal Path
- Configurable Adhesive and Sheet Formats
-
LAIRD TPLI220
- Thin 0.020-Inch Gap Filling
- 6.0 W/(m K) Interface Conductivity
- Optional One-Side Adhesive Formats
-
LAIRD TPLI220FG
- Fiberglass-Reinforced Thin Interface
- 6.0 W/(m K) Thermal Transfer
- Electrically Insulating Gap Filling
-
LAIRD TPLI240
- Compliant 0.040-Inch Gap Filling
- 6.0 W/(m K) Thermal Path
- Configurable Adhesive Interface Formats
-
LAIRD CFS-8480
- Broad RF Absorption Capability
- Flexible Castable Processing
- Elevated-Temperature Electrical Performance
-
LAIRD CR-110
- Above 26 GHz Absorption Range
- 100:16.5 Controlled Mixing
- Below 180 deg C Service Temperature
-
LAIRD CR-114
- 10 to 14 GHz Absorption Range
- 100:6.5 Controlled Mixing
- Below 180 deg C Service Temperature
-
LAIRD CR-116
- 6 to 12 GHz Absorption Range
- 100:4.3 Controlled Mixing
- Below 180 deg C Service Temperature
-
-
LAIRD CR-124
- Below 5 GHz Absorption Range
- 100:2.6 Controlled Mixing
- Up to 150 deg C Service Temperature
-
LAIRD CR112
- 12-to-18-GHz Absorber Grade
- Castable Two-Part Epoxy System
- Molded and Localized RF Absorption
-
LAIRD CRS-117
- Flexible RTV Silicone Microwave Absorber
- 100:1.18 Controlled Mixing
- 0.9 W/(m K) Thermal Conductivity
-
LAIRD CRS-124
- Flexible RTV Silicone Microwave Absorber
- 100:1.00 Controlled Mixing
- 1.0 W/(m K) Thermal Conductivity