PLEXUS MA8110
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 1:1 Controlled Mixing
- 9 to 11-Minute Working Window
- 24.8 MPa Cured Tensile Strength
Product Description
PLEXUS® MA8110 Methacrylate Adhesive is a two-part, 1:1 methacrylate structural adhesive for direct bonding to many metal substrates, including galvanized G60 and G90 steel, and for selected thermoplastic and composite assemblies. The gray, non-sag mixed adhesive provides a typical 9 to 11 minute working time at 23°C and supports gap-filling bondlines from 0.75 to 9.5 mm. It is documented for limited surface preparation on supported substrates and develops high tensile and lap-shear properties after cure.
Key features
- Direct-to-metal bonding: The adhesive is documented for primerless bonding to many metals, including galvanized G60 and G90 steel.
- 9 to 11-minute working time: The documented process window is measured at 23°C.
- Gap-filling cured bond: The adhesive supports 0.75 to 9.5 mm bondlines with typical tensile strength of 21.4 to 24.8 MPa.
Applications / Suitable for
- Structural bonding of galvanized and other metal assemblies
- Selected thermoplastic bonding
- Composite assembly bonding
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color, Part A | Off-white | N/A | As supplied |
| Color, Part B | Gray | N/A | As supplied |
| Mix ratio | 1:1 | parts by volume | Part A : Part B |
| Mix ratio | 1:1 | parts by weight | Part A : Part B |
| Viscosity, Part A | 40,000 to 70,000 | cP | As supplied |
| Viscosity, Part B | 40,000 to 70,000 | cP | As supplied |
| Working time | 9 to 11 | min | At 23°C |
| Shelf life | 7 | months | Stored at 12 to 23°C |
After-processing / final-state properties
Typical final-state values under the stated conditions. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Recommended bondline gap | 0.75 to 9.5 | mm | Documented range |
| Tensile strength | 21.4 to 24.8 | MPa | ASTM D638 |
| Tensile modulus | 690 to 900 | MPa | Typical cured value |
| Tensile strain | 10 to 20 | % | Typical cured value |
| Lap shear strength | 12.4 to 15.8 | MPa | ASTM D1002 |
| Operating temperature range | -40 to 82 | °C | Documented range |