ECCOBOND FP4547

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND FP4547

Main features

  • Enhanced adhesion
  • Rigid, low stress seal
  • High purity

Product Description

LOCTITE ECCOBOND FP4547 liquid epoxy underfill is designed to provide enhanced adhesion to integrated circuit passivation materials. This material is formulated to quickly underfill devices at 90 to 120°C substrate temperature, with as little as a 2 to 3 mil gap.

When fully cured, the material forms a rigid, low stress seal that dissipates stress on solder joints and extends thermal cycling performance. LOCTITE ECCOBOND FP4547 also exhibits low moisture absorption for improved JEDEC performance.

Recommended Cure Schedule

  • 30 minutes @ 165°C
Product Family

221988

10 cc - Syringe
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 50 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Syringe
Net weight 16 g
Gross weight 27 g
Dimensions 2 x 10.5 x 3.2 cm
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
135 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
18,000 mPa.s