DOWSIL 3-1965
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- One-part silicone conformal coating
- Flexible cure options: room temperature or heat-accelerated
- Wide operating temperature range (-55°C to 200°C)
Product Description
DOWSIL™ 3-1965 Conformal Coating is a one-part, no-added-solvent silicone conformal coating designed for protective coating of printed circuit boards and electronic assemblies. It provides very low viscosity (approximately 115 cP) for excellent flow into fine features and complex geometries, cures at room temperature through exposure to atmospheric moisture, and can be heat-accelerated to support manufacturing efficiency. Once cured, it forms a soft, flexible elastomer that provides electrical insulation, environmental protection, and stress relief for sensitive electronic components and densely populated PCB designs, subject to application-specific testing and qualification.
Key features
- Very low viscosity - ~115 cP enables excellent flow into tight spaces, fine-pitch components, and complex PCB geometries.
- Moisture-cure RTV system - Cures at room temperature through exposure to atmospheric moisture with optional heat acceleration.
- No-added-solvent formulation - Helps reduce process complexity and supports cleaner coating operations.
- Soft elastomer after cure - Low-stress silicone material helps protect sensitive components and solder joints.
- Excellent coverage performance - Flows easily under and around densely populated electronic assemblies.
- Electrical insulation properties - Provides reliable dielectric protection for PCB assemblies.
- UV indicator - Enables inspection and verification of coating coverage under UV light.
Applications
DOWSIL™ 1-2620 Low VOC Conformal Coating is suitable for electronics assemblies where low-viscosity silicone coating, circuit-board protection, and coating inspection are part of the application review.
- Rigid and flexible circuit boards: suitable for protective coating of printed circuit boards and PCB system applications.
- PCB assembly protection: supports environmental protection, corrosion resistance, and dielectric protection requirements.
- Printed Wiring Boards (PWB): low-viscosity flow is required to ensure uniform coverage of circuit traces, solder joints, and component leads
- Sensitive electronics and fine-pitch designs: suitable for tightly spaced geometries where low-viscosity flow is required to achieve uniform coverage.
Related resources
TDS, SDS & Technical Documents
Technical Specifications
No specifications available.
Additional Information
DOWSIL™ 3-1965 RTV Coating
DOWSIL™ 3-1965 Conformal Coating is a one-part, transparent, no-added-solvent silicone conformal coating designed to protect printed circuit boards and electronic assemblies from moisture, corrosion, thermal cycling, and environmental contaminants. The coating features a low viscosity of approximately 115 cP, cures at room temperature through exposure to atmospheric moisture, and can be heat-accelerated to support manufacturing efficiency.
Review the technical data sheet and SDS before handling, processing, or qualifying the material.

Silicone Conformal Coating for Electronic Protection
DOWSIL™ 3-1965 RTV Coating cures upon exposure to atmospheric moisture, eliminating the need for solvent evaporation during processing. Its room-temperature cure can be accelerated with mild heat to support faster production cycles. The coating's high-viscosity, self-leveling formulation is suitable for a range of application methods and provides consistent coverage of electronic assemblies.
As a cured elastomer, DOWSIL™ 3-1965 RTV Coating delivers excellent flexibility and low-modulus properties, helping to minimize mechanical stress on sensitive components, solder joints, and interconnections during thermal cycling and environmental exposure.
Key features
- Room-temperature cure - Cures through solvent evaporation followed by silicone crosslinking.
- Solvent-free formulation - 100% solids silicone system with no solvents or by-products.
- Low viscosity coating - Supports spray, dip, and selective coating application methods
- Flexible elastomer after cure - Shore A 33 material reduces mechanical stress on sensitive components and solder joints.
- UV indicator - Facilitates inspection and verification of coating coverage under UV light.
- Reliable environmental protection - Provides resistance to moisture, corrosion, and contaminants in harsh environments.
Processing summary
Product Documents and Dow Coating Resources
Review the technical data sheet for typical product properties, the safety data sheet for handling and storage requirements, and the Dow conformal coatings selection guide for broader context on the coating family.
Use the selection guide to compare DOWSIL™ conformal coating options by viscosity, cure profile, hardness, and agency listing context.
The Dow conformal coatings selection guide explains how silicone coatings are positioned by viscosity, cure profile, hardness, stress relief, abrasion resistance, UV inspection, and agency listing context. It also includes a solventless coating section for applications where reducing solvent-handling complexity is a key selection driver, along with comparison tables for solventless RTV, solventless heat-cure, and solvent-based RTV conformal coatings.
Performance Properties
Cure basis and test conditions are per technical data sheet unless otherwise stated.
| Property | Typical value | Unit |
|---|---|---|
| One or Two Part | One | |
| Color | Translucent | |
| Viscosity | 115 0.1 |
cP Pa-sec |
| Specific Gravity (Cured) | 0.99 | |
| Tack-Free Time at 25ºC | 6 | minutes |
| Durometer Shore A | 34 | |
| Dielectric Strength | 425 17 |
Volts/mil kV/mm |
| Volume Resistivity | 8.7 E14 | ohm-cm |
| Dissipation Factor at 100 Hz | 0.001 | |
| Dissipation Factor at 100 kHz | < 0.0002 | - |
| UL Flammability Classification | 94 V-0 | - |
| Mil Specification | Mil I-46058C Amend 7 | - |
| Agency Listing | IPC-CC-830 with Amendment 1 |
- |
| Cyclotetrasiloxane (D4) content | < 0.1 | % |
Where DOWSIL™ 3-1965 fits
Tips and troubleshooting
| Issue | Recommended action |
|---|---|
| Air entrapment or voids |
|
| Adhesion below target |
|
| Curing |
|
| Moisture exposure during storage |
|
| Repair or rework requirement |
|
Frequently asked questions about DOWSIL™ 3-1965 RTV Coating
What is DOWSIL™ 3-1965 RTV Conformal Coating used for?
It is used to protect printed circuit boards and electronic assemblies from moisture, corrosion, and environmental contaminants while providing electrical insulation and long-term reliability, especially in fine-pitch and densely populated designs..
How does this coating cure?
DOWSIL™ 3-1965 RTV Coating cures by atmospheric moisture at room temperature. Mild heat can be used to accelerate processing after sufficient solvent flash-off.
Which application methods are supported?
DOWSIL™ 3-1944 RTV Coating can be applied through brush, flow coat, or needle/dispense. Process fit should be confirmed against the target wet-film thickness, board layout, masking approach, and keep-out areas.