ABLESTIK TE3530

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK TE3530

Main features

  • One component
  • Thermally conductive
  • Low viscosity

Product Description

LOCTITE ABLESTIK TE 3530 adhesive is designed for bonding heat dissipation components and can be applied by automatic syringe dispense. It cures at moderate to low temperatures allowing it to be used on heat sensitive materials.

LOCTITE ABLESTIK TE 3530 is a white, thermally conductive epoxy adhesive with low temperature cure that is typically used in sensor and die attach assemblies. Operating temperature is 150°C.

Cure Schedule

  • 30 minutes @ 100°C or
  • 15 minutes @ 120°C or
  • 10 minutes @ 150°C

Technical Specifications

Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
2.3 W/m.K
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
60,000 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers