ABLESTIK 8290

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 8290

Main features

  • Low bleed
  • Low stress
  • Improved JEDEC performance

Product Description

LOCTITE® ABLESTIK 8290 electrically conductive die attach adhesive is designed for high reliability leadframe packaging applications. It is recommended for die sizes smaller than 5mm for the best MRT performance.

LOCTITE® ABLESTIK 8290 is an epoxy based, silver filled, heat curable adhesive with low bleed and low stress that also achieves improved JEDEC performance.

 

Cure Schedule

  • 30 minute ramp to 175°C + 15 minutes @ 175°C
Product Family

8290/10C0

10cc Syringe - 1200408
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 55 days
Packaging
Unit of measure Syringe
Net weight 38 g
Gross weight 47 g
Dimensions 3 x 2.3 x 9.2 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Thermal Properties
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
8 W/m.K
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
4.0
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
16,000 mPa.s

Leading Brands Trust in Our Products and Services