ABLESTIK 3880

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 3880

Main features

  • One component
  • Thermally and Electrically conductive
  • SMD bonding

Product Description

LOCTITE ABLESTIK 3880 is designed for bonding of metals, ceramics, rubbers and plastics as used in electronic parts, where good adhesion combined with electrical and thermal conductivity is required. Typical applications include bonding surface mount devices to flexible or rigid substrates, bonding of semiconductor elements, joining EMI parts, bonding electrodes, lead wires or other connectors that require conductivity.

LOCTITE ABLESTIK 3880 is a monocomponent, thermally and electrically conductive adhesive that can be used to mount electronic components via syringe and stencil print.

Cure Schedule:

  • 10 minutes @ 125°C
  • 6 minutes @ 150°C
  • 3 minutes @ 175 °C
Product Family

221896

5 cc - Syringe | Silver Gray
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 23 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Unit of measure Syringe
Net weight 10.6 g
Gross weight 20 g
Dimensions 2.8 x 1.8 x 7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.4
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
40 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
2 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0008 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
50,000 mPa.s

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers