ABLESTIK 2114

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 2114

Main features

  • Optically Clear Bonding
  • 50 N/mm^2 Cured Tensile Strength
  • Broad Metal/Glass/Ceramic/Plastic Compatibility

Product Description

LOCTITE ABLESTIK 2114 BIPAX is a two-component, transparent, non-conductive epoxy adhesive supplied in a BIPAX mixing-dispenser package for easy mixing. Formulated for optical clarity and low viscosity, it is recommended for industrial adhesive and laminating applications. This solvent-based system cures at room temperature over 24 hours or with an accelerated schedule, and supports continuous service from -60°C to 110°C. It bonds metals, glass, glass fabrics, ceramics, and plastics, offering strong tensile strength, good electrical insulation, and environmental and chemical resistance in its cured state.

Key features

  • Transparent with optical clarity: Low viscosity and refractive index of 1.57 for optically clear bonding applications.
  • High tensile strength: 50 N/mm² (7,200 psi) tensile strength in the cured state.
  • Electrically insulating: Dielectric strength of 410 volts/mil supports non-conductive assembly needs.

Applications / Suitable for: Industrial adhesive and laminating applications across metals, glass, glass fabrics, ceramics, and plastics.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Transparent
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.57
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.17
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
640 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
77 °C
Operating Temperature
-60 to 110 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
3.5000000000 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured, mixed material prior to cure.

Property Value Unit Method / condition
Viscosity, mixed 640 mPa·s (cP) @ 25°C, mixed
Specific gravity, mixed 1.17 — Mixed material
Pot life 60 minutes Mixed material
Technical properties

After-processing / final-state properties

Typical properties of the fully cured material after the recommended cure schedule.

Property Value Unit Method / condition
Hardness 78 Shore D Cured material
Glass transition temperature (Tg) 77.0 °C Cured material
Dielectric strength 410 volts/mil Cured material
Tensile strength 50 (7,200) N/mm² (psi) Cured material
Lap shear strength, Al to Al 16.2 (2,350) N/mm² (psi) Sample cured 1 hr @ 100°C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers