3M™ Resealable Loop and Hook Fastener SJ352D

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M™ Resealable Loop and Hook Fastener SJ352D

Main features

  • Provide a firm adhesive bond to a wide variety of surfaces
  • Durable for thousands of closures
  • Best suited for indoor use

Product Description

3M™ Reclosable Fastener SJ352D is a durable nylon hook-and-loop fastening system designed for quick, reliable attachment across a wide range of applications. Coated with a high-performance rubber adhesive, it provides strong bonding to various substrates, including paper, metals, glass, and plastics. This system offers a practical solution for applications requiring repeated opening and closing, helping improve efficiency and reduce production time. The product includes both hook (SJ3526N) and loop (SJ3527N) components and is best suited for indoor use.

Product Key Features

  • Nylon fastener allows easy, repeatable opening and closing
  • Rubber-based adhesive adheres well to a wide variety of surfaces
  • Designed to withstand thousands of fastening cycles
  • Performs up to 50°C long-term and 70°C short-term
  • Bonds to paper, cardboard, metals, glass, painted surfaces, wood, and many plastics
  • Quick fastening reduces assembly time and labor costs
  • Suitable across multiple industries and applications
  • Includes both hook and loop components for immediate use

Applications

  • General fastening in transportation, electronics, and office equipment
  • Shopfitting and display assembly
  • Mounting signage and indoor fixtures
  • Securing panels, covers, and lightweight components
  • Packaging and temporary holding applications
  • Projects requiring repeated attachment and removal
Product Family

234947

Black, 25 mm x 5 m, 4.4 mm, Dispenser Box
1. Select Width
2. Select Length
3. Select Thickness
4. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Box
Net weight 0.5 kg
Gross weight 0.5 kg
Dimensions 33.5 x 23 x 5 cm

Technical Specifications

General Properties
Color
The color
Black
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
3600 μm