3M DP100FR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Scotch-Weld™ Epoxy Adhesive DP100FR

Main features

  • Fast cure
  • Easy mixing
  • • Meets UL 94 V-0

Product Description

3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 minutes after mixing. It is ideal for many applications requiring a self-extinguishing structural epoxy adhesive system.

Product Key Features

  • Fast cure
  • Easy Mixing
  • Meets UL 94 V-O (File No. E61941)
  • Passes 14 CFR 25.853 (60 Sec. Vertical Burn Test: As listed in code Federal Regulations, FAA, DOT Regulations 25.853 paragraph a.)
  • Does not contain brominated or antimony-based flame retardants.
Product Family

204245

48.5 mL - Cartridge | Off White
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 0.090718 kg
Gross weight 0.090718 kg
Dimensions 4.61 x 2.57 x 12.08 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Epoxy
Color
The color
Cream
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
1:1
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
61 °C

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers