3M 7240FR
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Long open time for large surface application
- Non-sag properties
- Contains glass beads for thickness control
Product Description
3M™ Scotch-Weld™ Epoxy Structural Adhesive 7240 B/A FR is a two-part, 2:1 mix ratio adhesive and contains glass beads for control of minimal bond line thickness.
Product Key Features
- Long open time for large surface application
- Non-sag properties
- Contains glass beads for thickness control
- High resistance to environmental exposure
Technical Specifications
General Properties
Chemistry Type
Modified Amine/Modified Epoxy
Color
White/Black
The color
Work life @25°C
1 hours
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate.