3M 100
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Short-Term Exposure to 232 deg C
- Metal and High-Surface-Energy Plastic Adhesion
- Low-Outgassing Tape Construction
Product Description
3M High Temperature Acrylic Adhesive 100 is a pressure-sensitive acrylic adhesive system used in transfer tapes for bonding metals and high-surface-energy plastics. It combines solvent resistance with shear resistance at elevated temperatures. In transfer-tape constructions, short-term temperature resistance extends to 232 deg C for minutes or hours, while longer exposures can reach 149 deg C for days or weeks. The adhesive system has low outgassing and low levels of leachable chlorides. Transfer-tape constructions pair it with different adhesive thicknesses and release liners for electronics, aerospace, and die-cutting applications.
Key features
- Short- and long-term heat exposure: Adhesive 100 supports temperatures up to 232 deg C for minutes or hours and up to 149 deg C for days or weeks in transfer-tape constructions.
- Pressure-sensitive acrylic bonding: The adhesive bonds metals and high-surface-energy plastics in transfer-tape constructions.
- Low-outgassing adhesive system: Transfer-tape constructions combine low outgassing with low levels of leachable chlorides.
TDS, SDS & Technical Documents
Technical Specifications
Other Properties
Electrical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Construction and roll dimensions vary by tape grade. Caliper values are calculated from controlled coat weights and are stated as typical construction data, not performance specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive caliper - Tapes 941, 965, 966, 9462P | 2.3 (0.06) | mil (mm) | Calculated from manufacturing-controlled adhesive coat weights; density 1.012 g/cc. |
| Adhesive caliper - Tape 9461P | 1.16 (0.03) | mil (mm) | Calculated from manufacturing-controlled adhesive coat weights; density 1.012 g/cc. |
| Release liner - Tape 941 | 58# polycoated Kraft; 4.0 | mil | Construction listed in TDS. |
| Release liner - Tape 966 | 62# densified Kraft; 3.8 | mil | Printed liner; construction listed in TDS. |
| Release liner - Tapes 965 and 9462P | 55# densified Kraft; 3.2 | mil | Printed liner; construction listed in TDS. |
| Release liner - Tape 9461P | 55# densified Kraft; 3.2 | mil | Printed liner; construction listed in TDS. |
| Core size | 3 | in | Paper core. |
| Standard roll length | 180 | yd | TDS lists standard length. |
| Available width | 1 to 48 | in | Minimum width is 3 in for Tape 9462P; 1 in for other listed tapes. |
After-processing / final-state properties
The following static-shear values are representative or typical only and must not be used as specifications. They apply to bonded samples under the stated load, duration, and substrate conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Static shear - room temperature | 2,000 g for 10,000 | g / min | All Adhesive 100 family tapes; stainless steel; 1 × 1 in test samples. |
| Static shear - 158°F (70°C) | 1,000 g for 10,000 | g / min | All Adhesive 100 family tapes; stainless steel; 1 × 1 in test samples. |
| Static shear - 200°F (93°C) | 1,000 g for 10,000 | g / min | All Adhesive 100 family tapes; stainless steel; 1 × 1 in test samples. |
| Static shear - 350°F (177°C) | 500 g for 10,000 | g / min | All Adhesive 100 family tapes; stainless steel; 1 × 1 in test samples. |
| Static shear - 450°F (232°C) | 400 g for 10,000 | g / min | All Adhesive 100 family tapes; stainless steel; 1 × 1 in test samples. Tape 965 showed some slippage above 200°F (93°C). |